Synthesis and characterization of ferroelectric bismuthtitanate (Bi4Ti3O12)

dc.contributor.authorBalram
dc.contributor.supervisorSingh, Dwijendra P.
dc.date.accessioned2013-10-16T07:15:17Z
dc.date.available2013-10-16T07:15:17Z
dc.date.issued2013-10-16T07:15:17Z
dc.descriptionMaster of Scienceen
dc.description.abstractThe Lead free, Bismuth Titanate (BIT) has been synthesized by Sol-Gel method. The synthesized samples have been subjected to the structural, morphological, hysteresis measurements. The X-Ray Diffraction studies have confirmed that Bismuth Titanate (Bi4Ti3O12) have the orthorhombic phase without any impurity peak in XRD data. The SEM studies have shown the good surface morphology with varying clusters ranging from 0.5μ to 1μ. The SEM micrograph of BIT indicates that each and every clusters appearing on the surface is comprised of large no. of crystallites. The hysteresis measurement of BIT is also done to confirm the ferroelectric property of the material. The value of Pr and Ec in hysteresis loop is affected by the externally applied field for the drawing the P-E loop. For the higher field, these values are higher as compare to the lower applied electric field (at 12KV/cm2, Pr = 0.14451μC/cm2, Ec = 5.597KV/cm and at 10KV/cm2, Pr = 0.12070μC/cm2, Ec = 4.6456 KV/cm).en
dc.description.sponsorshipSchool of Physics and Materials Science, Thapar University, Patialaen
dc.format.extent1330246 bytes
dc.format.mimetypeapplication/pdf
dc.identifier.urihttp://hdl.handle.net/10266/2649
dc.language.isoenen
dc.subjectFerroelectricen
dc.subjectsol-gelen
dc.titleSynthesis and characterization of ferroelectric bismuthtitanate (Bi4Ti3O12)en
dc.typeThesisen

Files

Original bundle

Now showing 1 - 1 of 1
Loading...
Thumbnail Image
Name:
2649.pdf
Size:
1.27 MB
Format:
Adobe Portable Document Format

License bundle

Now showing 1 - 1 of 1
Loading...
Thumbnail Image
Name:
license.txt
Size:
1.79 KB
Format:
Item-specific license agreed upon to submission
Description: