Concrete is one of the most widely used construction materials. However, the formation of microcracks during service allows the ingress of water and aggressive substances, resulting in deterioration and reduced durability. Microbially induced calcium carbonate precipitation (MICCP) has emerged as a promising approach for developing self-healing concrete. However, the use of Kombucha-derived bacterial cellulose (BC) as both a reinforcing material and a carrier for self-healing bacteria remains relatively unexplored. The present study investigated the development and application of bacterial cellulose as a carrier and reinforcement material in concrete. Bacterial cellulose was produced through Kombucha fermentation using a sugar and tea-based medium. The cellulose sheets were harvested, purified using 1 N NaOH, washed, dried at 55°C, and processed into coarse fibres. The morphology and elemental composition of the produced BC were characterized using Field Emission Scanning Electron Microscopy coupled with Energy Dispersive X ray Spectroscopy (FE-SEM-EDX), while its crystalline structure was analysed using X-ray diffraction (XRD). The BC was subsequently incorporated into concrete at 0.3%, 0.5%, and 0.7% of cement weight. In addition, Bacillus megaterium SS3 was immobilized onto BC fibres using a bacterial suspension of 5 CFU/mL for 2 h, and the bacteria-loaded fibres were incorporated into concrete at the same concentrations. Concrete cube specimens were prepared and cured in nutrient broth. Compressive strength was evaluated at 7 and 28 days, while water absorption was evaluated after 28 days. FE-SEM analysis revealed a distinct interconnected three-dimensional fibrous network with visible pores and spaces characteristic of bacterial cellulose. EDX analysis showed carbon and oxygen as the major elements, with average mass percentages of 66.64% and 27.47%, respectively. XRD analysis showed characteristic peaks at approximately 14.5°, 16.7°, and 22.6°, consistent with the crystalline Cellulose I structure. Among the concrete formulations, 0.3% bacteria-loaded BC exhibited the highest compressive strength, reaching 21.56 MPa at 7 days and 35.75 MPa at 28 days, compared with 18.48 MPa and 28.83 MPa, respectively, for the control. Increasing BC concentration beyond 0.3% did not result in further improvement in compressive strength. Water absorption was 4.45% for the control, while bacteria-loaded BC specimens showed lower values of 3.58%, 3.62%, and 3.80% at 0.3%, 0.5%, and 0.7% BC, respectively. The 0.3% bacteria-loaded BC specimen showed approximately 19.6% lower water absorption than the control. Overall, the findings demonstrate the potential of Kombucha-derived bacterial cellulose as a multifunctional material for concrete, providing reinforcement potential while serving as a carrier for self-healing bacteria. The 0.3% bacteria-loaded BC formulation showed the most favourable combination of compressive strength and water absorption among the formulations investigated. However, direct evaluation of crack healing, microscopic confirmation of calcium carbonate precipitation, bacterial viability after incorporation, and long-term durability are required to establish the self-healing performance of the developed system more comprehensively.

Description

Citation

Endorsement

Review

Supplemented By

Referenced By